> Could someone be kind enough to tell me > what is the minimum distance between the > edge of pcb and the end of pad on a > panelized board ? IPC -std ? > We do not use IPC standards here but we use .040" from the board edge if it's scored and .020" if it's routed. I personally feel that's waaaaay too much real estate to throw away but it wasn't my decision. Anyone care to help me get this changed? All help is appreciated. Happy Holidays! *<():-)> JoAnn L. Amerson Design Librarian Red Lion Controls, Inc. E-mail: [log in to unmask] Voice: (717) 767-6961 ext 6308 ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ##############################################################