Charles Barker@I-O INC 12/04/97 10:32 AM Steve, We experienced a somewhat similar problem a while back. Some parts were falling off the bottom of the boards prior to wave soldering. Usually, but not always, the parts were close to the edge of the board. We found two problems. Some of the adhesive being used was past its expiration date. We were doing pin transfer at that time and we found that it would sometimes be left in the "pot" and used past its "window" of time (hours) of usefullness after exposure to air. Once those areas were addressed and people were educated, the problem went away. We never did get into measuring the pull strength, although we talked about it. Please respond to [log in to unmask]; Please respond to [log in to unmask] To: [log in to unmask] cc: (bcc: Charles Barker/IO-US) Subject: [TN] Gen: Soldermask Adhesion What is the typical adhesion factor (Bonding Strength) for soldermask to the bare copper surface? Will there be a difference in the shear factor number? <Snip> Has anyone else encountered similar opportunities in the past and if so what were the conclusions? Steve Collins PCB Design Supervisor ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ##############################################################