I have used the Elcometer 345 Digital Coating Thickness Gauge with satisfaction. By the specification, the accuracy is * 5 % or 0,1 mil. The gauge is to measure coatings on thick metals, but in can be calibrated to measure coatings on thin materials like copper foil on PWB. Manufacturer is Elcometer Instruments Ltd in England. I believe you will find a supplier in your country. Jarmo Kiiski [log in to unmask] > -----Original Message----- > From: Yuen, Mike [SMTP:[log in to unmask]] > Sent: 4. joulukuuta 1997 0.37 > To: [log in to unmask] > Subject: [TN] Ultrasonic Guage > > Does anyone out there have any GOOD EXPERIENCE with any non-contact > thickness gauge for measuring conformal coating (1 to 10 mils)? > > Thanks, > Michael Yuen > [log in to unmask] > > ############################################################## > TechNet Mail List provided as a free service by IPC using LISTSERV > 1.8c > ############################################################## > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in the body: > To subscribe: SUBSCRIBE TECHNET <your full name> > To unsubscribe: SIGNOFF TECHNET > ############################################################## > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for > additional information. > For the technical support contact Dmitriy Sklyar at [log in to unmask] or > 847-509-9700 ext.311 > ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ##############################################################