What if any are the repercussions of clearing solder out of via holes with a laser? Would there be barrel damage due to localized heating effects? (6 layer,1.59mm thick pcb, 0.343mm via hole) What should we be looking for? Any test results documented? Background- Solder mask openings for the vias were added for prototypes by their cam operator, but when moved to the production facility, this procedure was not transferred. First shipments (thousands) had no solderball problems even though vias had no openings for the LPI soldermask (Enthone DSR3241 I believe). Pcb's were reflowed with no components or paste to ascertain if it was an assembly issue. Many large solder balls appeared. There are approximately 800 vias on the board and apparently, it takes about a minute to clear the via holes out each board with the laser. Cheers, [log in to unmask] ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ##############################################################