DON'T use 1/0 laminate! Take 1/1 laminate and coat 1 side with resist and etch off the uncoated side! Fred J. >>> FULABHAI <[log in to unmask]> 12/05/97 12:09pm >>> Laminate .062 10/1 is not industry standard , means not easily available. Better to make your own in your shop using copper sheet of desired thickness ! This kind of copper sheets available in market. coppersheet-18 mil (with brown oxide) + 2 x 1060 pre-prag + . 040 0/1 laminate and go in press... Be careful in drilling... and Etching... It works.. Fulabhai, [log in to unmask] Ph. (408)972-1456 ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ##############################################################