We have been using Kester 244 no-clean solder paste on cards with Entek 56 and 106 OSP's for a couple of years or so now, with no problems to date. Regards Evan Evan Jones Manufacturing Engineer IBM Wangaratta Ph 61 3 5720 2539 Fax 61 3 5720 2412 Email [log in to unmask] ---------------------- Forwarded by Evan Jones/Australia/IBM on 01/12/97 16:15 --------------------------- [log in to unmask] 29/11/97 08:21 Please respond to [log in to unmask] @ internet To: [log in to unmask] @ internet cc: Subject: [TN] Entek Plus 106 and Kester no clean flux 951 Is anyone using Enthone, Entek plux 106 and Kester no clean flux 951 (2% solid content) and solderpaste? I'd like to get some inputs from users of Entek plux and no clean flux/paste for smt/mixed boards. Thanks Matthew ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ##############################################################