Matthew, I have had some experience with Kester 951 and have had some problems using it in our process with very high impedience circuits. Have not had any problems with lower impedience circuits (less than 100K ohms). Never used Entek. Regards Paul Matthew Park wrote: > Is anyone using Enthone, Entek plux 106 and Kester no > clean flux 951 (2% solid content) and solderpaste? > I'd like to get some inputs from users of Entek plux and no > clean flux/paste for smt/mixed boards. > > Thanks > Matthew > > ############################################################## > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c > ############################################################## > To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: > To subscribe: SUBSCRIBE TECHNET <your full name> > To unsubscribe: SIGNOFF TECHNET > ############################################################## > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. > For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 > ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ##############################################################