Poh, If you are putting TSOPs on FR-4 and temperature cycle them you are going to have problems, no matter how good your joints look. The thermal coefficient of expansion mismatch between the part and board is so great that you will quite often find that the TSOPs will "unzip" their joints along one entire side! Bev Christian Nortel ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ##############################################################