Hi Tenison, If you have investigated pad geometry in terms of your tombstoning problem, you should have found that smaller is better. Your solder fillets are too large. Reduce the pads extension beyond the component ends and you will find the tombstoning disappear. Narrowing the pads is also a good move. Werner Engelmaier Engelmaier Associates, L.C. Electronic Packaging, Interconnection and Reliability Consulting 23 Gunther Street In December: 7 Jasmine Run Mendham, NJ 07945 Ormond Beach, FL 32174 USA Phone & Fax: 973-543-2747 Phone: 904-437-8747, Fax: 904-437-8737 E-mail: [log in to unmask] ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ##############################################################