Lately we received boards from one of our PCB suppliers with gold fingers that look "oxydised". Does anybody know what could be the root cause of gold fingers looking like that. They are dark yellow, sometimes uniform, sometimes stained. It comes off when we "erase" them with a white eraser. Is it a bad rinsing and/or bad drying after plating ? Could it be the gold itself that is a poor quality ? What would be the impact on functionality ? Is there any ? Thanks in advance for any feedback AL ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ##############################################################