I am looking for a printable peelable mask which can withstand three thermal cycles. The mask can be no more than 3 mils thick when cured. All of the ones that I tried worked well with two thermal cycles. But when they were exposed to three, either they became to difficult to remove, showed evidence of cracking, or stained the board. Thanks Mike Yuen ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ##############################################################