To clarify the information request. Carbon filled Teflon was being used as boats, in a cleaning process, for small parts. In the process the carbon was redepositing on the parts and interfering with further processing. The switch to carbonless Teflon caused ESD to be an issue (significant static charges). Looking for range of 10 to 8th - 10 to 4th surface resistively. Also have to withstand cleaning solutions from acids to bases and high temperatures. Semper Fi Tom >---------- >From: Lepsche, Thomas G (NM75) >Sent: Wednesday, November 05, 1997 10:11 AM >To: [log in to unmask] >Subject: Teflon replacement > >Technetters, > >Does anyone know of a high temperature, conductive (low surface resistively), >chemical resistant plastic (no carbon) that can be substituted for Teflon. > Is there a company that specializes in this type of plastic? > > Thanks for your help! >Semper Fi >Tom > ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ##############################################################