Mary Why not ask your PC Fab supplier to make them with your production batches? If you are intending to do SIR tests, you MAY get misleading info if the coupon is from a different source than your normal fabricator - and there may be some ageing issues to think about. Graham Naisbitt Concoat Ltd Email: [log in to unmask] Alasan House, Albany Park Tel: +44 (0)1276 691100 Camberley, Surrey GU15 2PL UK Fax: +44 (0)1276 691227 -----Original Message----- From: TechNet On Behalf Of Davis, Mary Sent: Wednesday, November 26, 1997 9:43 PM To: [log in to unmask] Subject: [TN] Source for MIL-I-46058 Y Pattern Coupons I'm looking for a source for 'off the shelf' Y pattern test coupons. Any help you can give will be greatly appreciated. Mary Davis Hughes Aircraft Co. Naval & Maritime Systems 425-356-3311 ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ##############################################################