Hi Jan: We have seen cases where pcbs which passed at low voltage subsequently showed shorts at higher voltage. When retested at lower voltages the shorts were still present indicating that the board had changed due to the higher voltage stressing. This was traced to fibers which were present due to a problem with etching bath temperatures. Don Hague Luther & Maelzer 781-275-4560 ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ##############################################################