Why the blast on J-leads? We've been using them for years in high thermal cycle environments on FR-4 boards with little or no problems. I was just wondering if you had some data that we didn't possess that would lead us to reevaluate our use of these parts? Thanks Max Bernhardt Woodward Governor Co. ---------- From: Bob Vanech To: [log in to unmask] Subject: Re: [TN] J-Lead Mods