When the TH part is inserted the past in the hole does get pushed out but the extra paste around the pad is pulled in by capillary action. We have not tried this yet but intend to try a few test boards. Pete Holden Coin Acceptors [log in to unmask] ############################################################## IPC Designers Council Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE DESIGNERCOUNCIL <your full name> To unsubscribe: SIGNOFF DESIGNERCOUNCIL ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ##############################################################