Ken: Some of the rules for minimum distance between holes and board edge were developed for punching or shearing. The mechanical stresses from those operations would fracture the laminate if holes were too close to the edge. Using CNC drilling and routing, the main concern is to provide sufficient annular ring for component soldering and to provide for manufacturing tolerances so a hole near the board edge doesn't become half a hole. Nonplated holes breaking out of the board edge are frequently used in some designs. Partial (half) holes that are plated thru can work well if the board edge is also plated. (100% edge plating and board removal from a break-away scheme can be challenging.) Reliable holes with plating that break out of the board edge are extremely challenging if edge plating and burrs are not allowed. Don Vischulis Ken Patel wrote: > Is there any spec. on drilling a plated hole non-plated hole form the edge, > I mean, what is the safest minimum distance a hole can be drilled from the > edge. I believe thickness of the board is a one factor. > > Re, > Ken Patel > ______________________________________________________ > Ken Patel Phone: (408) 490-6804 > 575 Cottonwood Dr. Fax: (408) 490-6859 > Milpitas, CA 95035 Beeper: (888) 769-1808 > > ############################################################## > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c > ############################################################## > To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: > To subscribe: SUBSCRIBE TECHNET <your full name> > To unsubscribe: SIGNOFF TECHNET > ############################################################## > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. > For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 > ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ##############################################################