Hello Denis, Could you be more specific about the chemistry, operating parameters and plating additive used ? Regards, Charles Desroches Technical Advisor ViaSystems Canada inc. > ---------- > From: Dennis Rice[SMTP:[log in to unmask]] > Reply To: TechNet Mail Forum.;Dennis Rice > Sent: Thursday, October 09, 1997 1:14 PM > To: [log in to unmask] > Subject: [TECHNET] SMUTTING > > WE HAVING BEEN HAVING TROUBLE WITH OUR ANODES LOSING SMUT. COULD > SOMEONE > GIVE ME THE CAUSES WHY THIS COULD HAPPEN WITH A TREATED BATH AND NEW > ANODES AFTER DUMMY PLATING. THIS IS AN ON GOING PROBLEM. > > THANKS > DENNIS RICE > > ############################################################## > TechNet Mail List provided as a free service by IPC using LISTSERV > 1.8c > ############################################################## > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in the body: > To subscribe: SUBSCRIBE TECHNET <your full name> > To unsubscribe: SIGNOFF TECHNET > ############################################################## > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for > additional information. > For the technical support contact Dmitriy Sklyar at [log in to unmask] or > 847-509-9700 ext.311 > ############################################################## > ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ##############################################################