I' would like to inciate an open discusion about "copper electroless vs DMT". If DMT have lower consumption of chemicals, panel to panel uniformity, more productivity and big economy in rinse water without mention the enviromental efects, why the mayority of the PCB's manufacturers are using copper electroless? Does anybody think that DMT is going to replace copper electroless in a few time or not? Eduardo Tovar ############################################################## IPC Designers Council Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE DESIGNERCOUNCIL <your full name> To unsubscribe: SIGNOFF DESIGNERCOUNCIL ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ##############################################################