Rob: Could you quantify "moderately rough"? -- Warren Szkolnicki Process Engineer Broadband Networks Inc, 37 Stevenson Road, Winnipeg, MB, CANADA R3H 0H9 email: [log in to unmask] ph: (204) 982-8480 x 229 fax: (204) 982-8487 WWW: http://www.broadbandnetworks.com Robert Schetty wrote: > The data that I've seen on this subject indicates that very > smooth Ni/Au > surfaces wire bond poorly. On the other hand, an extremely rough > Ni/Au > surface also exhibits poor wire bond pull strengths. In general, it > seems a > "moderately rough" Ni/Au surface provides the best results. > > Rob Schetty > LeaRonal Inc. > > ---------- > ---------- > ------------------------------------------------------------------- > ------------------------- > A question came up on what the surface finish (smoothness/roughness) > should > be for wire bond on a land. The plated finsh is typically nickel and > a > covered with a soft gold finsh. Will hills and valleys in the surface > make > any difference in the bond strength. > > Phil Hinton > hintpwb1@aol,com