Charles, Send me your fax number and I will forward the two documents to you. I tried to Email them to myself and the files got corrupted. I assume you had the same problem. Denis At 10:42 AM 8/26/97 -0500, you wrote: >Charles Barker@IO-US >08/26/97 10:42 AM > >Do any of have and, if so, would you be willing to share, any statistics >you may have on amount of solder used per joint in the wave soldering >process? We are trying to project how much solder in bar form should be >needed for different volumes of boards/joints. > >Thanks in advance. > >