Tamir, Try Circuit Repair Corporation at www.circuitnet.com or email @ [log in to unmask] 45 Research Drive Haverhill, MA 01832-1293 Phone 508-374-5000 They can either sell you the supplies you need for your people to do the repair, or you can send them the assemblies, and they can do the work for you. Bill Spalton ------------- Original Text From Tamir Ben-Shoshan <[log in to unmask]>, on 8/3/97 9:11 AM: To: <[log in to unmask]> Hello, Since the increasing of using BGA the need for pad reconstruction were rise. I need some details about a companies that produce or supply such reconstruction kit, the size of the pad are 30 mil. Thanks tamir.