Cristian Bomboe wrote:- >Hi TechNet, > >Which is the best protection for gold plated edge conectors to be applied before >HAL? > >Thanks, >Cristian Hello Christian, We have found tape to be the best answer although you can use peelable solder mask. Tape can be cut to size before application or applied along the complete edge. We have tried various tapes and can recommend one in particular. If you would like to e-mail me direct I can give you the details. The main thing with any mask is to cover the gold completely and overlap onto solder mask or laminate. If solder gets a touch of the gold it will wick up under the mask as it dissolves the gold. Also, try to HAL with the edge connectors on the vertical edge. Paul Gould Teknacron Circuits Ltd [log in to unmask] Isle of Wight,UK