Hi Matt - Copper and Copper oxide are both plain copper but two entirely different beasts. Proof of this is the great oxide discussions relating to wedge voids that have hit Technet the last few days. The impact of the state of copper oxide reduction is very important in the board fabrication process which other Technetees can better describe than I. Dave Hillman Rockwell Collins [log in to unmask] ______________________________ Reply Separator _________________________________ Subject: Re[2]: Part II: Mechanism of Wedge Void Formation Author: [log in to unmask] at ccmgw1 Date: 7/16/97 9:45 PM Then again, the reduced oxide is supposed to be plain copper, isn't it? Matt Byrne HADCO-Owego ______________________________ Reply Separator _________________________________ Subject: Re: Part II: Mechanism of Wedge Void Formation Author: [log in to unmask] at SMTPLINK-HADCO Date: 7/16/97 07:59 AM Hi TechNet - There is a tool available that can very accurately measure both the type and the quantity of copper oxide present on a surface in a nondestructive manner - Sequential Electrochemical Reduction Analysis (SERA). The ANSIJ-STD-003 PWB solderability committee recently completed a gauge R&R study on several SERA equipments and is in the process of submitting the test method for inclusion in the IPC-TM-650 specification. Although the 003 committee's focus is on solderability, the SERA test method can also evaluate copper surface oxides. Contact the folks at ECI Technologies (201-773-8686) for more information. Use of this method could be used to eliminate the subjectiveness or as a supplement to copper oxide identification by visual appearance. Dave Hillman Rockwell Collins [log in to unmask] ______________________________ Reply Separator _________________________________ Subject: Part II: Mechanism of Wedge Void Formation Author: [log in to unmask] at ccmgw1 Date: 7/15/97 5:14 PM Rudy Sedlak mentions that a reduction in oxide thickness from black to brown to red in color assists in deterring wedge voids. This trend could lead to a cosmetic difficulty. Am I correct? Matt Byrne states that reduced oxide helps: Here I take this to be reduction from cupric to cuprous ions which Rudy Sedlak confirms. Richard Fudalewski states that reduced oxide brings in a problem of its own, but I am uncertain which definition that Sedlak mentioned he is referring. **** New question: At what minimal thickness does one entertain cupric ion post oxide reduction with DMAB? What are the trade offs cosmetically versus functionality (w.r.t. wv's)? Again thanks, Josep P.S. In direct answer to Byrne's question of reduction problem, we see wv problems intermittently. The goal is to strive for a cosmetic black coating. Thickness entering DMAB is typically 0.28mg/cm2 (black not brown before immersion). Acid resistance (10% HCl) is greater than 2 hours. These wv issues are not related to layer counts. I cannot as yet pin the mechanism down but have not ruled out materials such as prepreg. I'd like to understand more about the contact mechanism of prepreg during lamination, whether other's verify Tg of lots, and if this has ever been an issue in wv troubleshooting. [log in to unmask] *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************