Phil - Brass is copper/zinc and so the zinc is still there. The kinetics of the oxide reaction on large copper areas are usually enough to overcome the galvanic cell set up with the zinc but not always. There is a way to fix. Please contact me off-line. Roger Mouton INSULECTRO 714-587-3216 *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************