You can have problems with wave soldering after BGA component placement, and you have the correct concerns. This is sometimes a design dependant issue -- how much heat do you transfer through the vias... via size, cross section, Cu thickness all have affects. Most assembly shops will not only use LPI plugs on the back side of the bga area, but they also tape them off with kapton tape. I recommend you thermal couple the board under the bga and run some through your wave process and look for reflow temperatures on the BGA side of the board. That's the safest way to know if you are OK> Stay as cool as you can and still get good reflow/solder joints on the solder side of the board. Hope that helps. Jim Herard KBL, Product Quality Engineering IBM Microelectronics Endicott t/l 857-7026 ---------------------- Forwarded by Jim Herard/Endicott/IBM on 07-16-97 05:33 PM --------------------------- [log in to unmask] 07-16-97 10:56 AM Please respond to [log in to unmask] @ internet To: [log in to unmask] @ internet cc: Subject: Wave and BGA Hello all, I will like to have comment on any effect that a wave can do on a BGA. We have some boards with BGA on component side and many component on the solder side. Our process will be reflow component side, glue solder side, install all TH parts and go to wave. Is anyone had or have problems with BGA (solder joints problem) after wave? Our via's are half tented with solder masks and the trace connecting the via to the BGA pad is approx. 0.020"-0.030". My concerns are: - Re-reflow of BGA solder ball causing cold solder or any solder defect? - Reliability problems? - Etc. Any advice will be well appreciated. Thank you. Andre Bisson CAE Electronics [log in to unmask] *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************