Most aqueous LPI solder masks on the market are mixtures of epoxy resin systems with acrylate resins/monomers. The acrylates react quickly to free radical type polymerization (initiated by UV radiation) through the double bonds (as you stated). The epoxy resin does give desirable properties, such as electrical insulation, chemical resistance, toughness, etc. There are some all epoxy LPI masks on the market. The most common are the Probimer 52 type solvent developed products from Ciba-Geigy. They use different type photoinitiation systems and are very slow reacting (often taking minutes) in typical UV type exposure units. I am not aware of all acrylate LPI mask, but I suppose these would be possible. Overall properties would probably not be quite as good as the ones with epoxy resins in the system. Hope this helps. Larry Fisher Dexter Electronic Materials [log in to unmask] *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************