Sheldahl, Inc. may be able to help you. There address and phone number are: Sheldahl, Inc. 1150 Sheldahl Road Northfield, Minnesota, USA 55057-9444 Phone: 507-663-8000 Fax: 507-663-8545 Contacts: Bruce Olson, Brent Sweitzer, or Sidney Roberts >>> guerard <[log in to unmask]> 07/22/97 11:01am >>> We need polyimide flexible jumpers for nuclear detector feedthrough fabrication. The geometric specifications are as following : number of conductive lines : 36 pitch : 1 mm (distance between the axis of twoo adjacent lines) width of a line : 0.5 mm length of the flexible : 300 mm materials : the conductive lines are inserted between 2 polyimide foils. contacts : lines are ended by a contact on both sides for soldering. We are interested by any similar product (but different for one or more of our parameters) that would avoid the tooling charge. Does anybody a company that might have such products. Thank you very much _/ _/ _/ Bruno Guerard _/ _/ _/ email:[log in to unmask] _/ _/ _/ Institut Laue-Langevin _/ _/ _/ B.P.156, 38042 Grenoble Cedex 9, France _/ _/_/_/_/ _/_/_/_/ tel:(33) 76.20.72.77 fax:(33)76.20.77.00 *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************