Dan, Can you use UV light or perhaps chlorine? Jill steeper at Shipley in Marlborough, MA knows about this stuff, give her a call. Chuck Brummer ______________________________ Reply Separator _________________________________ Subject: Biocide, no formaldehyde. Author: [log in to unmask] at ccUnix Date: 7/17/97 11:06 AM To: TechNet We have a mildly acidic citrate type plating bath that develops MOLD after periods of unuse, usually within two to three weeks. The mold stains the deposit and plugs the filters. We prefer not to use formaldehyde as a biocide due to its toxicity. Can anyone recommend a benign biocide? Please advise. Daniel Brandler, Ohmega Technologies, [log in to unmask] *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************