While I applaud the logic in saying that the post drilling wet processes only expose the problem and are not the cause, I believe the logic should be taken one step farther. If you look at the drilling process, it is difficult to visualize a .0135" diameter drill (that will break if you look at it cross-eyed) pulling layers apart. Consider also that the stack is clamped with a pressure foot before the drill touches the stack. I believe that drilling is very seldom the cause, rather it plays almost the same role as the post drilling wet processes by exposing the layer to layer join in the hole wall. Also, my experience has been that wedge voids and pink ring will happen on only one layer (possibly two) and not on the others in the same panel. Again, it's difficult to imagine a drill bit selectively wedge voiding a hole wall at one specific point in the panel especially when the drilling takes place in a two or three high stack. *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************