I would like to know what the required hold down time is for vacuum lamination prior to loading into the press. We currently still use turkey bags and hold vacuum for 30 minutes, which is how long the press takes to heat up for each cycle. On some of the newer presses that have vacuum chambers, the press is loaded immediately, especially if is a hot press only. What is the criteria for this process? Any thoughts on this would be greatly appreciated. Thanks. *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************