How can I find out more information about SERA? ______________________________ Reply Separator _________________________________ Subject: Re: Re[2]: Solder Mask Residue Author: [log in to unmask] at corp Date: 7/16/97 2:56 PM SERA is Sequential Electrochemical Reduction Analysis. The technique can detect and quantify the oxides and other reducible species on the metal and alloys surfaces. The presence of the soldermask residue can be monitored on the copper too. Regards Mike Pavlov *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************