I'm not sure the exact technical name or the content of this glue. It is widely use for shoe repair and wood work. Normally we put the glue on both surface, leave for 10-15 minutes, then paste together. I think it is rubber base. The problem is how to remove this glue from the concrete floor. The previous tenants who occupy this office drop patches of this glue on the floor, some as thick as one inche. It has been accumulated for sometime and harden. We tried to use Toluene. But toluene just dissolve it slightly and made the hard glue become sticky. Is there any chemicals/solvent that could dissolve this glue fast and effective? Else I've to contunue with chisel and hammer! Regards Mohd Misri N.Sembilan. *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************