Sam, I''m not sure about "everyone else" but I have never heard of HAL over the tin plating. Now , I can't back this next statement up with any written document or study but... It would seem to me that by introducing tin plated surfaces repetitively could eventually affect the SnPB composition ratio in the solder pot as well as the coated surfaces. On the surface tt just doesn't sound like a good practice for the HAL process. Ed Cosper Graphic Electronics Inc. Tulsa OK ---------- From: sam mccorkel[SMTP:[log in to unmask]] Sent: Tuesday, June 10, 1997 12:29 PM To: [log in to unmask] Subject: Tin / HASL Is it an accepted practice to tin plate ( for an etch resist ) and then hot air solder level over the tin? We're considering this for SMOTL finishes but have concerns about the tin plated boards going into the HAL. Does anyone know if we're asking for trouble or do other manufacturer's do the same? *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************