I recommend you thermocouple the ceramic, and also have it checked for moisture content. Something seems wrong. I'd expect the solder joints to fail before the ceramic if its a thermal expansion stress problem. You could have a bad batch of ceramics. Also, you may want to look at columns instead of balls. Jim Herard IBM Microelectronics Quality Engineering ---------------------- Forwarded by Jim Herard/Endicott/IBM on 06-12-97 05:38 PM --------------------------- ssmith @ ael.com 06-11-97 05:22 PM Please respond to [log in to unmask] @ internet To: TechNet @ ipc.org @ internet cc: Subject: FEB: ceramic BGA cracking after wave solder We are experiencing cracking of large (1.8" on a side) ceramic BGA cracking (like in half) following wave solder. The devices are on polyimide boards. This is a new program -- any advice on things we might do better or different ... bake the boards before we stuff them? fixture boards during wave solder? go back to our board supplier for resolution? Thanks for any help... Sheila Smith, Tracor AES *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************