With regards to the many inquires regarding the selectively removal of Liquid Photoimageable Solder Mask (LPISM) from PCBs. SolderMask, Inc. has developed the ability to selectively remove LPISM and Dry Film Solder Mask from bare PCBs. It in some cases the processes MAY work on partially or fully populated boards. If you are interested please contact Frank Kurisu, at (714) 842-1987. Regards, Frank Kurisu -----Original Message----- From: Blanchet,Richard Sent: Thursday, June 19, 1997 6:40 AM To: ipc Subject: FW: removing solder mask Let's say CM2001 from Grace and a selective removal for example. ---------- From: TechNet-request To: TechNet Subject: Re: removing solder mask Date: 19 June, 1997 08:47 Paul: There has been much discussion lately on Technet about just this issue, and what it boils down to, is what is the soldermask, and do you want selective, or general removal? Rudy Sedlak RD Chemical Company *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************