>To: [log in to unmask] >From: [log in to unmask] >Subject: Resin Removal > >We are currently producing large quanties of blind via panels on standard FR4 materials. This is causing a bottleneck at our resin removing operation, prior to drilling, and I have been asked look at a more efficient method. > >Our current procedure is Plasma desmear after bonding followed by a light brush prior to drilling. > >We have evaluated PTFE and other proprietary blocking films during the bonding operation, but have found them to be too expensive,or they create other problems due to 'dish down' at the via enterance. Allowing the resin to flow onto the surface has proved the most effective method at this time. > >I would be intrested to hear how other manufacturers remove resin from blind via panels, and if they have any comments or suggestions on the procedure stated above. > >yours in anticipation > >Billy Shaw > >Process Engineering Manager > >Thomas Walter, Marlow, England, UK > > *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************