Denis Meloche wrote:- >Does anyone have information on how to repair gold edge connectors which >have solder on them? I remember a product or service from the late 70's or >early 80's which purported to fix this. Can anyone shed some light on the >subject? I have seen the defect repaired by reflowing with Au80/Sn20 but I >am unsure of the long term reliability of this method. >Thanks, Hi Denis, A repair system comprising a small rectifier and plating pen is the best answer. The tin lead will have to be stripped chemically or mechanically and the affected contacts re-plated. You will need to mask the contacts with a suitable tape, strip the tin-lead, then make the contact cathodic while plating with the anodic pen and swab containing the gold solution. Sound preparation is critical to getting good adhesion and the plating repair system should come complete with solutions and instructions to do this. It is not as difficult as it sounds. Don't forget to check the adhesion of the gold with a tape test. Oddly enough, I had a visit from a supplier last week and one of their products was just such a system. If you are unable to locate a supplier, email me and I will be happy to give you the details. -- Paul Gould Teknacron Circuits Ltd [log in to unmask] Isle of Wight,UK *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************