Not many shops carry G10 as most of the work being done needs to be UL approved and G10 doesn't cut it. In fact, it may be difficult to get the old stuff now anyway. When the bromine was added years ago, it made plated thru holes very difficult until people realized the change and chemical changes of the deposition process had to be made. *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************