To measure a squeegee's hardness you should purchase a "Shore A Durometer." Instructions usually come with the device. One source of durometers is Midwest Sign & Screen Print Their number is: 1-800-824-2468. Hope that helps ______________________________ Reply Separator _________________________________ Subject: Gen- Durometer Measurement Author: [log in to unmask] at corp Date: 5/29/97 7:51 AM Date 29/5/97 Subject Gen- Durometer Measurement >From Maurice Dore To Technet Gen: Durometer Measurement Hi all, Any chance anyone can advise me on how to measure the shore/durmoeter value for a squeegee for screen printing. Any IPC references? Again, thanks in advance. Rgds M *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************