Thanks for the reply on ultrasonic cleaning. Another question for boards soldered with a rosin based rosin flux. Present cleaning solution utlrasonic is 75% isopropyl 25% DI water with a few drops of Triton X-100 a nonionic surfactant, and a final rinse in alcohol and water with a dwell time of 30-45 seconds in the ultrasonic. Is this a good choice or is there better. The rosin (actually resin) based flux is applied during hand solding and would normally would not need to be completely removed, but operating temperatures around 200deg C may cause charring and possibe conductance. *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************