Jim, For true conductor protection, all exposed surfaces must be coated. If conductive liquids bridge the gap between balls of different potentials you've got trouble. So, this would seem to dictate vertical dipping as the only reliable means of coating. But, the coating must not be allowed to remain in the space between the board and the device, after dipping, due to high relative thermal expansion mismatch of solder and cured acrylic. The opinions expressed herein are not necessarily those of my employer. Lyn R. Lynch Coates ASI ______________________________ Reply Separator _________________________________ Subject: ASSY: CONFORMAL COATING BGAs Author: [log in to unmask] at internet Date: 6/26/97 9:18 AM Does anyone have any experience applying conformal coating on an assembly which contains BGA components? Is it necessary to ensure that all solder joints are coated? If so, how it it done and how is it verified? My specifics are: Military contract 625 ceramic BGA .030" stand-off Acrylic coating Any opinions will be welcome. Thanks, Jim Marsico (516) 595-5879 [log in to unmask] ******************************** * ______ _ _ _____ * * / ___ | | | | | _____ * * / /___| | | | | | _____ * * __/ ____ | | | | |______ * * |____/ |_| |_| |________| * * * * SYSTEMS, INC. * ******************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************