we are repacking the devices immediately after removing the devices required for use same day.Use desicator packs and sealing machine. Add on vacuum cleaner for creating vacuum before final seal. We found this method quite useful and economical. The exposure of devices while devices are being removed from packings is so short to affect any performance at RH levels of 30-40%. ---------- From: Snider, Scott/NTSEUG To: 'IPC Technet' Subject: FW: Dry Storage Date: Monday, June 02, 1997 4:05PM I'm looking for alternative ways to store moisture sensitive components once the vapor barrier bags are opened. We currently don't use N2 in our facility and would like to avoid using it in this application. Any suggestion of manufacturer's. We only need about 3 - 5 cubic feet storage. *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************