You are right , Glenn Making a 2113 (or 2313) prepreg is no problem and it works fine as a prepreg BUT it makes a really awful laminate for the reasons you have stated. ---------- From: [log in to unmask] To: [log in to unmask]; [log in to unmask]; Dave Heywood Subject: re: RE: Re:FAB Prepreg style 2113 Date: 26 May 1997 09:54 <<File Attachment: ENVELOPE.TXT>> I'd be careful requiring 2113 or 2313. If I remember right, and please somebody correct me if I'm wrong, these two styles have unbalanced weaves. The filament weight in one direction is heavier than in the other (in addition to the fiber count difference). This has made it harder to run through a treater, more broken filaments from weaving and impregnating (results in etching problems), uneven movement for dimensional stability, and different surface profiles in grain and fill. From the weavers end, I think it was being phased out and replaced by a balanced weave, although I don't remember the number. Glenn Pelkey Quality/Reliability Engineer Maxtek Components Corp. [log in to unmask] Wrote: | | 2113 is used a lot in Europe where it more or less replaces 2125 as a 4 mil prepreg. It presses | maybe a smidgeon thinner but not much (depending on the resin content favoured by your local | supplier). The only downside is that it has almost the same thread count as 2116 and is therefore | difficult to distinguish visually. this can lead to confusion and the odd mistake among companies that | employ humans. | Dave Heywood | [log in to unmask] | ---------- | From: [log in to unmask] | To: [log in to unmask]; Dave Heywood | Subject: Re:FAB Prepreg style 2113 | Date: 21 May 1997 03:08 | | We are after typical build uses of style 2113 prepreg. | | Any help would be appreciated. | | Regards, | David Taylor | Chief Engineer | East Coast Printed Circuits *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************