From: Scott Westheimer Date: 5/14/97 Recently we encountered a problem with adhesion of the S/M during HAL. We use Giba's S/M and due to some problems we have to processing boards through HAL several times to get all of the areas covered with solder. We tried several things to try to improve the adhesion and have found two that seem to work well. A 3% H2SO4 dip prior to ALO3 scrub and skipping the UV bump until after HAL have given us excellent results. Our QA department has concerns about the properties of the S/M with UV bumping after HAL and I was wondering if any has tried this approach and if they have found any problems with doing this. Also we are considering putting the H2SO4 directly in the ALO3. Any comments? *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************