Richard, We currently use Dow Corning 1753 silicon conformal coat with the Nordsen select coat system (we also use an inline spray system). We have not had any problems with this, its been a very good coat for us. Please call if you want more specifics (or contact Dow Corning, as they have done case studies on us). Chris Messner UT Electronic Controls 219-358-3429 ______________________________ Reply Separator _________________________________ Subject: Assy: conformal coating Author: "Blanchet;Richard" <[log in to unmask]> at Internet Date: 5/28/97 9:51 AM Hello, I'm looking for any information concerning solvent-free conformal coating application process (products, articles, advices, suppliers, experience, etc.). Thank you. Richard Blanchet Canadian Marconi [log in to unmask] *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************