Richard, We are presently using Dow 3-1765, which is a solvent free silicon. We are applying this coating with a Nordson Select Coat. I would be more than willing to discuss our application with you off-line. Gary Camac Dickey-john Corp. 217-438-2288 [log in to unmask] ______________________________ Reply Separator _________________________________ Subject: Assy: conformal coating Author: INTERNET:[log in to unmask] at CSERVE Date: 5/28/97 9:52 AM Sender: [log in to unmask] Received: from kani.wwa.com (kani.wwa.com [198.49.174.58]) by arl-img-5.compuserv e.com (8.6.10/5.950515) id JAA06358; Wed, 28 May 1997 09:52:07 -0400 Resent-Date: Wed, 28 May 1997 09:52:07 -0400 Received: from ipc.org/ipc.ipc.org [209.42.29.23] by kani.wwa.com with smtp (Smail3.2.WWA) id m0wWj86-003rR9C; Wed, 28 May 1997 08:51:24 -0500 (CDT) Received: by ipc.org (Smail3.1.28.1 #2) id m0wWiyc-000BjMC; Wed, 28 May 97 08:41 CDT Resent-Sender: [log in to unmask] Old-Return-Path: <[log in to unmask]> Date: Wed, 28 May 1997 09:51:00 -0400 (EDT) From: "Blanchet,Richard" <[log in to unmask]> Subject: Assy: conformal coating To: ipc <[log in to unmask]> Message-Id: <338C385F@srvsmtp> Mime-Version: 1.0 Content-Type: TEXT/PLAIN; CHARSET=US-ASCII Resent-Message-ID: <"vRbir2.0.EiB.wN3Zp"@ipc> Resent-From: [log in to unmask] X-Mailing-List: <[log in to unmask]> archive/latest/12961 X-Loop: [log in to unmask] Precedence: list Resent-Sender: [log in to unmask] Hello, I'm looking for any information concerning solvent-free conformal coating application process (products, articles, advices, suppliers, experience, etc.). Thank you. Richard Blanchet Canadian Marconi [log in to unmask] *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************