Hi Chuck - You might try giving Inco Alloys a phone call (304-526-5570) and talk with the technical staff about plating to Monel. They may be able to help. Dave Hillman Rockwell Collins [log in to unmask] ______________________________ Reply Separator _________________________________ Subject: Plating over Monel Author: [log in to unmask] at ccmgw1 Date: 5/23/97 10:37 AM Anybody out there plate other metals over Monel? We are trying to plate Ni/Au over a thin layer of Monel. This Monel is protecting a very thin copper layer. When we plate to the copper side the adhesion is good. When we plate the Ni then gold to the Monel side it peels or fails the tape test. Anybody got any ideas? I appreciate the help and thanks in advance. Chuck Brummer Acuson AIM (818) 734-4930 *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************