Phil, make that 14 Gig. :-) (the guy down the hall from phil), dwight At 12:42 PM 5/1/97 -0700, Phil Bavaro wrote: >Our assemblies operate as high as 12 GHz with no problems over the last >five years of no clean assembly. > >Phil >----- > > >At 12:07 PM -0400 4/30/97, Brian Bauer wrote: >>Hello, >> >>Does anyone have any information on the effect of no clean residues on RF. >>I am interested at what frequency interference begins (if any) and what type >>of device you are talking about ie. phine, radio etc.. I am interested in >>both PCB and Hybrid Thick Film (alumnia) applications. Also, is anyone using >>no cleans in the Gigahertz level - if so what level? >> >>Thanks >> >>Brian >> >>*************************************************************************** >>* TechNet mail list is provided as a service by IPC using SmartList v3.05 * >>*************************************************************************** >>* To subscribe/unsubscribe send a message <to: [log in to unmask]> * >>* with <subject: subscribe/unsubscribe> and no text in the body. * >>*************************************************************************** >>* If you are having a problem with the IPC TechNet forum please contact * >>* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * >>*************************************************************************** > > > >*************************************************************************** >* TechNet mail list is provided as a service by IPC using SmartList v3.05 * >*************************************************************************** >* To subscribe/unsubscribe send a message <to: [log in to unmask]> * >* with <subject: subscribe/unsubscribe> and no text in the body. * >*************************************************************************** >* If you are having a problem with the IPC TechNet forum please contact * >* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * >*************************************************************************** > > > *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************