5/16/97 GEN: H2O Bake out 12:40 PM Hello everybody: We are trying to determine if a moisture removal bake is necessary for hand (soldering iron) and/or automated (screen print/vapor phase) multilayer PWB assembly. If baking is required, then what conditions should be used (time, temp, vacuum, etc.)? What influence does extended storage under ambient conditions (60%R.H. 70oF) have? Does anyone use a drybox for storage? Once boards entered the assembly area (and baked - if necessary), how long before a re-bake is required? We primarily use Type GIN glass/polyimide materials for passive chip SMT. Boards that get assembled within a few days after fabrication would probably NOT require a bake, but we have to allow for extended storage - up to 5 years from date of manufacture. Thank you in advance for any help Gino Cochella (310) 814-3955 TRW Inc. *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************